Vehicle recall 19 March 2018

Ford Focus and C-max recall: Casting defect may cause alloy wheel(s) to crack

Yes – some of these vehicles are being recalled
What's wrong
A small batch of alloy wheels may have a casting defect that may initiate a fatigue crack and result in wheel failure.
What to do
Contact a Ford dealer to book the free repair. Check wheels on affected vehicles for a specific batch code. Replace those wheels which have the identified batch code.
Source: Driver and Vehicle Standards Agency (DVSA) Check your reg on DVSA ↗

What’s wrong

A small batch of alloy wheels may have a casting defect that may initiate a fatigue crack and result in wheel failure.

The fix

Check wheels on affected vehicles for a specific batch code. Replace those wheels which have the identified batch code.

Vehicles affected

Model Built from Built to Vehicles
Focus 26 Sep 2016 10 Oct 2016 80
C-max 26 Sep 2016 10 Oct 2016 80

How to check your vehicle

Use the official DVSA checker with your registration number to see if your exact vehicle is included. If it is, the manufacturer should have written to the registered keeper. The repair is free, even if you bought the vehicle second-hand.

Updated 19 March 2018. This page summarises an official notice. Details can change – always follow the official notice.